posted on Tuesday, December 8, 2020 A version of this article by Dr. Edward Rolinski was written for and originally appeared in Industrial Heating's November 2020 issue.
View More
posted on Thursday, September 17, 2020 Die failures are caused by complex wear mechanisms at the surface of the die cavity. Surface properties critical for die performance can be improved by a novel surface-treatment process employing a multi-gradient design strategy.
posted on Thursday, August 8, 2019 This article originally appeared in Industrial Heating, November 2015. Scroll below to learn more about improving stamping dies with ion/plasma nitriding.