posted on Friday, December 11, 2020 An aerospace/defense customer was experiencing galling and excessive wear on their foil blade forging dies. AHT helped them to significantly improve their shot count with ion nitriding.
View More
posted on Wednesday, August 19, 2020 Read how AHT was able to help the US Military with their heat treat needs...
posted on Wednesday, September 6, 2017 Advanced Heat Treat Corp. Receives Significant Nadcap Achievement