Long/Large Parts

Advanced Heat Treat Corp.'s UltraGlow® Nitriding is your answer to an economical way of heat treating rolls, shafts, extruder screws, and much more.

Nitrided Tie Bar

Long and/or large parts processed in the finished condition benefit from UltraGlow® Ion Nitriding and Gas Nitriding because they require precise control of the nitrided structure, dimensional stability, and a minimized need for polishing after treatment.

Offered in the states of Alabama, Iowa & Michigan, Advanced Heat Treat Corp.'s nitriding / nitrocarburizing equipment can accommodate heat treat needs up to:

  • 160" in diameter

  • 360" in length

  • 60,000 lbs. in weight

Plus, we have large size capabilities for additional processes such as blasting, stress relieving, tempering, age hardening and UltraOx®.  


Nitriding Long Parts

Advanced Heat Treat Corp.'s Monroe, Michigan facility specializes in the ion (plasma) nitriding of very LONG parts, and we've captured the longest part we've ever nitrided on video! This team effort truly shows how Advanced Heat Treat Corp. goes "above" and beyond to exceed customer expectations with UltraGlowing results!

Learn more about AHT's abilities to nitride long and large parts like feedscrews in our article, "Enhancing Plastic Extruder Screws Performance with Nitriding." 